Polymer Property : Adhesive Bond Strength = 23.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 23.0 MPa

@Temperature -55.0 °C
3340 psi

@Temperature -67.0 °F
Lap Shear
Henkel Hysol PL 696 Film Adhesive
Epoxy-based structural film adhesive designed primarily for out-of-autoclave curing process applications requiring low cure temperatures as well as low curing pressures and is also available in ligh..