Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 29.7 MPa @Temperature 25.0 °C |
4310 psi @Temperature 77.0 °F |
Lap Shear |
Henkel Hysol PL 795-1 Film Adhesive Tougher version of Hysol PL 795. Excellent flow characteristics. Excellent tack and handling characteristics. Improved elevated temperature performance. Can be used for both surfacing film and light.. |