Polymer Property : Adhesive Bond Strength = 3030 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 20.9 MPa

@Thickness 1.50 mm
3030 psi

@Thickness 0.0591 in
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203); EN 1465
Dow BETAMATE™ 1045 Epoxy
BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent..