Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow BETAMATE™ 1045 Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Dow Chemical
Trade Name BETAMATE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow BETAMATE™ 1045 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent after gelling) Readily pumped at moderate temperatures Excellent adhesion to automotive steels, including coated steels and pretreated aluminum Resistant to degradation and substrate corrosion on environmental aging Compatible with electro-coat paint process in uncured state Information provided by Dow
Physical Properties Metric English Comments
Density 1.29 - 1.35 g/cc
0.0466 - 0.0488 lb/in³
Solids Content >= 99 %
>= 99 %
Viscosity 900000 cP

@Shear Rate 1.00 1/s,
Temperature 40.0 °C
900000 cP

@Shear Rate 1.00 1/s,
Temperature 104 °F
cone/plate
2.50e+6 cP

@Shear Rate 1.00 1/s,
Temperature 23.0 °C
2.50e+6 cP

@Shear Rate 1.00 1/s,
Temperature 73.4 °F
cone/plate
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 30.0 MPa
4350 psi
ISO 527-1
Elongation at Break 3.5 %
3.5 %
ISO 527-1
Modulus of Elasticity 2.50 GPa
363 ksi
ISO 527-1
Adhesive Bond Strength 13.6 MPa

@Thickness 0.750 mm
1970 psi

@Thickness 0.0295 in
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203); EN 1465
20.9 MPa

@Thickness 1.50 mm
3030 psi

@Thickness 0.0591 in
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203); EN 1465
Peel Strength 3.40 kN/m
19.4 pli
T-Peel (CRS St 1203, 0.5mm)
7.00 kN/m
39.9 pli
Impact Peel
Thermal Properties Metric English Comments
Flash Point >= 150 °C
>= 302 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 180 °C
0.500 hour

@Temperature 356 °F
Users viewing this material also viewed the following: