Polymer Property : Izod Impact, Unnotched (ISO) = 0.333 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 0.700 kJ/m²
0.333 ft-lb/in²
ISO R179
SABIC Innovative Plastics ULTEM Foam XP060 PEI
ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The ..
Izod Impact, Unnotched (ISO) 0.700 kJ/m² - NB
0.333 ft-lb/in² - NB
Average value: 43.4 kJ/m² Grade Count:274
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..