Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 0.700 kJ/m² | 0.333 ft-lb/in² | ISO R179 |
SABIC Innovative Plastics ULTEM Foam XP060 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Izod Impact, Unnotched (ISO) | 0.700 kJ/m² - NB | 0.333 ft-lb/in² - NB | Average value: 43.4 kJ/m² Grade Count:274 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |