Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 2.40 - 27.0 kJ/m² | 1.14 - 12.8 ft-lb/in² | ISO R179 |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compounding |
|||
Izod Impact, Unnotched (ISO) | 2.40 kJ/m² | 1.14 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® THD 121 Phenolic Compound, Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Izod Impact, Unnotched (ISO) | 2.40 kJ/m² | 1.14 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® THD 321 Phenolic Compound, Wood Flour & Cellulose, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & CelluloseApplications: Switchgear, HRC FusesProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industries Lt.. |
|||
Izod Impact, Unnotched (ISO) | 2.40 kJ/m² | 1.14 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® TX 321 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Electrical Properties Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |