Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 2.40 - 27.0 kJ/m² | 1.14 - 12.8 ft-lb/in² | ISO R179 |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compounding |
|||
Izod Impact, Unnotched (ISO) | 22.0 - 27.0 kJ/m² | 10.5 - 12.8 ft-lb/in² | Average value: 24.3 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 - 27.0 kJ/m² @Temperature -30.0 - -30.0 °C |
10.5 - 12.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 24.3 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |