Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 2.60 kJ/m² | 1.24 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® TMS 211 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |