Tipco Tipcolite® TMS 211 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength

Category Polymer , Thermoset , Phenolic
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolite® TMS 211 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ASTM D792
Apparent Bulk Density 0.420 g/cc
0.0152 lb/in³
TRM-37
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ASTM D638
Flexural Yield Strength 75.0 MPa
10900 psi
ASTM D790
Izod Impact, Unnotched (ISO) 2.60 kJ/m²
1.24 ft-lb/in²
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 5.01e+9 ohm-cm
5.01e+9 ohm-cm
ASTM D257
Surface Resistance 5.01e+8 ohm
5.01e+8 ohm
ASTM D257
Dielectric Strength 5.00 kV/mm
127 kV/in
ASTM D149