Polymer Property : Izod Impact, Unnotched (ISO) = 14.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 8.00 - 14.0 kJ/m²
3.81 - 6.66 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS02 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from television casings)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/gr..
Izod Impact, Unnotched (ISO) 8.00 - 14.0 kJ/m²
3.81 - 6.66 ft-lb/in²
Typical; ISO 180
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost..