Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 15.0 - 15.0 kJ/m² @Temperature -30.0 - -30.0 °C |
7.14 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 15.0 kJ/m² Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |