Polymer Property : Izod Impact, Unnotched (ISO) = 18.7 ft-lb/in² - NB Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 39.2 kJ/m² - NB
18.7 ft-lb/in² - NB
Average value: 87.4 kJ/m² Grade Count:25
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..