Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 42.0 - 42.0 kJ/m² @Temperature -30.0 - -30.0 °C |
20.0 - 20.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 42.0 kJ/m² Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL36P PC LNP* Lubricomp* DFL36P is a compound based on Polycarbonate containing 30% Glass Fiber 15% PTFE. Added features include: Exceptional Processing. Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RL4040HSUV PA 66 LNP* LUBRICOMP* RL4040HSUV is a compound based on Nylon 66 containing 20% PTFE. Added features of this grade include: Heat Stabilized, UV Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT LNP LUBRICOMP* WFL36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific) LNP LUBRICOMP* WFL36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI (Asia Pacific) LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 LNP STAT-KON* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF VF004S PA 66 LNP THERMOTUF* VF004S is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON MVL36SX0 PP (Europe-Africa-Middle East) LNP* VERTON* MVL36SX0 is a compound based on PP resin containing Long Glass Fiber and PTFE. Added features include: Chemically coupled, Heat Stabilized, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² @Temperature -30.0 °C |
20.0 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® HFD4412 PC Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Unnotched (ISO) | 42.0 kJ/m² | 20.0 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |