Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 88.3 kJ/m² | 42.0 ft-lb/in² | ISO 180 |
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(discontinu Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; .. |