Polymer Property : Izod Impact, Unnotched (ISO) = 88.3 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 88.3 kJ/m²
42.0 ft-lb/in²
ISO 180
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant  (discontinu
Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; ..