Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | ASTM D256 |
PTS PBT-20GFR 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by PTS LLC. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific) LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1eA |
Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled AS319L-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural or .. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL34EH PC LNP* LUBRICOMP* DFL34EH is a compound based on Polycarbonate containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Easy Molding, Healthcare, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific) LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 LNP* LUBRICOMP* SP003 is a compound based on Nylon 12 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific) LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² @Temperature 23.0 °C |
22.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su.. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON MD000A PP LNP* STAT-KON* MD000A is a compound based on Polypropylene resin containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear.. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DX06094 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DX06094 is a compound based on Polycarbonate resin containing Glass Fiber . Added features include: High Impact, Non- Brominated & Non-Chlorinated Flame Retardant and Mold Release... |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hGR40 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 LNP* THERMOCOMP* IC006 is a compound based on Nylon 6/12 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 (Asia Pacific) LNP* Thermocomp* IC006 is a compound based on Nylon 6/12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hXGR41 Polyphenylene Sulfide Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | ASTM D256 |
Tipco Tipcofil® AG 300 - 15% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 15% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 48.0 kJ/m² | 22.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON NV006E PC/ABS (Asia Pacific) LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |