Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP KONDUIT OTF2AXXP PPS (Asia Pacific)
LNP* Konduit* OTF2AXXP is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, Thermal Carbon Fiber. Added features of this material include: Thermally Conductive, Electrically C..
Izod Impact, Unnotched (ISO) 11.0 - 90.0 kJ/m²
5.23 - 42.8 ft-lb/in²
Average value: 73.9 kJ/m² Grade Count:16
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Unnotched (ISO) 11.0 kJ/m²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp WB006 PBT
LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starpylen MF007AS PP, Glass Fiber Filled, Injection Molded
Starpylen MF007AS is a Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 11.0 - 80.0 kJ/m²
5.23 - 38.1 ft-lb/in²
Average value: 31.5 kJ/m² Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..