Izod Impact, Unnotched (ISO) 1180 kJ/m²
561 ft-lb/in²
ASTM D4812
DuPont Performance Polymers Rynite® RE15022 NC010 Polyethylene Terephthalate (PET)
36% Glass Reinforced Polyethylene TerephthalateRynite RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performan..