Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 30.0 - 75.0 kJ/m² @Temperature -40.0 - -30.0 °C |
14.3 - 35.7 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 43.6 kJ/m² Grade Count:9 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 75.0 - 75.0 kJ/m² @Temperature -30.0 - -30.0 °C |
35.7 - 35.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 75.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |