Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 200 kJ/m²

@Temperature 23.0 °C
95.2 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1U
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66  (Unverified Data**)
Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf..
Izod Impact, Unnotched (ISO) 200 kJ/m²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 180-1U
Lanxess Durethan® BC 30 S 000000 Nylon 6
PA 6, non-reinforced, injection moldingInformation provided by LANXESS.
Izod Impact, Unnotched (ISO) 200 kJ/m²
95.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific)
Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys..
Izod Impact, Unnotched (ISO) 200 kJ/m²
95.2 ft-lb/in²
DAM; ISO 180/1U
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS BKB009 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productiv..
Izod Impact, Unnotched (ISO) 200 kJ/m² - NB

@Temperature -30.0 - -30.0 °C
95.2 ft-lb/in² - NB

@Temperature -22.0 - -22.0 °F
Average value: 250 kJ/m² Grade Count:5
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..