Polymer Property : Izod Impact, Notched (ISO) = 1.90 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.90 - 1.90 kJ/m²

@Temperature -40.0 - -40.0 °C
0.904 - 0.904 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 1.90 kJ/m² Grade Count:1
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..