Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polypropylene with 40% Mica Filler

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Mica Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polypropylene with 40% Mica Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.17 - 1.27 g/cc
0.0423 - 0.0459 lb/in³
Average value: 1.22 g/cc Grade Count:25
Filler Content 35.0 - 40.0 %
35.0 - 40.0 %
Average value: 39.5 % Grade Count:10
Water Absorption 0.0300 - 0.0400 %
0.0300 - 0.0400 %
Average value: 0.0367 % Grade Count:3
Linear Mold Shrinkage 0.00400 - 0.0130 cm/cm
0.00400 - 0.0130 in/in
Average value: 0.00719 cm/cm Grade Count:24
Melt Flow 2.00 - 17.0 g/10 min
2.00 - 17.0 g/10 min
Average value: 9.87 g/10 min Grade Count:19
Ash 40.0 %
40.0 %
Average value: 40.0 % Grade Count:9
Mechanical Properties Metric English Comments
Hardness, Rockwell R 33.0 - 104
33.0 - 104
Average value: 61.8 Grade Count:13
Hardness, Shore D 70.0 - 73.0
70.0 - 73.0
Average value: 72.0 Grade Count:4
Tensile Strength, Ultimate 14.0 - 32.4 MPa
2030 - 4700 psi
Average value: 26.4 MPa Grade Count:21
5.00 - 15.0 MPa

@Temperature 60.0 - 90.0 °C
725 - 2180 psi

@Temperature 140 - 194 °F
Average value: 10.0 MPa Grade Count:1
Tensile Strength, Yield 15.0 - 46.9 MPa
2180 - 6800 psi
Average value: 31.3 MPa Grade Count:14
Elongation at Break 3.00 - 10.0 %
3.00 - 10.0 %
Average value: 6.07 % Grade Count:15
5.00 - 20.0 %

@Temperature 60.0 - 90.0 °C
5.00 - 20.0 %

@Temperature 140 - 194 °F
Average value: 12.5 % Grade Count:1
Elongation at Yield 2.00 - 5.00 %
2.00 - 5.00 %
Average value: 2.83 % Grade Count:12
3.00 - 3.50 %

@Temperature 60.0 - 90.0 °C
3.00 - 3.50 %

@Temperature 140 - 194 °F
Average value: 3.25 % Grade Count:1
Modulus of Elasticity 2.50 - 4.83 GPa
363 - 700 ksi
Average value: 3.86 GPa Grade Count:12
1.20 - 2.50 GPa

@Temperature 60.0 - 90.0 °C
174 - 363 ksi

@Temperature 140 - 194 °F
Average value: 1.85 GPa Grade Count:1
Flexural Yield Strength 22.0 - 65.0 MPa
3190 - 9430 psi
Average value: 42.9 MPa Grade Count:15
Flexural Modulus 2.83 - 7.60 GPa
410 - 1100 ksi
Average value: 4.61 GPa Grade Count:25
Izod Impact, Notched 0.214 - 1.07 J/cm
0.400 - 2.00 ft-lb/in
Average value: 0.442 J/cm Grade Count:24
Izod Impact, Unnotched 1.60 - 5.34 J/cm
3.00 - 10.0 ft-lb/in
Average value: 2.76 J/cm Grade Count:7
Izod Impact, Notched (ISO) 1.90 - 1.90 kJ/m²

@Temperature -40.0 - -40.0 °C
0.904 - 0.904 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 1.90 kJ/m² Grade Count:1
Charpy Impact Unnotched 0.800 - 0.800 J/cm²

@Temperature -20.0 - -20.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.800 J/cm² Grade Count:1
Charpy Impact, Notched 0.100 - 0.100 J/cm²

@Temperature -20.0 - -20.0 °C
0.476 - 0.476 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.100 J/cm² Grade Count:1
Gardner Impact 0.300 - 2.26 J
0.221 - 1.67 ft-lb
Average value: 1.01 J Grade Count:8
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 - 149 °C
214 - 300 °F
Average value: 129 °C Grade Count:24
Deflection Temperature at 1.8 MPa (264 psi) 62.8 - 113 °C
145 - 235 °F
Average value: 85.4 °C Grade Count:21
Flammability, UL94 HB
HB
Grade Count:4
Processing Properties Metric English Comments
Nozzle Temperature 218 - 238 °C
425 - 460 °F
Average value: 229 °C Grade Count:5
Melt Temperature 191 - 249 °C
375 - 480 °F
Average value: 224 °C Grade Count:7
Mold Temperature 26.7 - 65.6 °C
80.0 - 150 °F
Average value: 43.5 °C Grade Count:8
Drying Temperature 65.6 - 90.0 °C
150 - 194 °F
Average value: 77.5 °C Grade Count:7
Moisture Content 0.0500 %
0.0500 %
Average value: 0.0500 % Grade Count:4
Injection Pressure 2.76 - 103 MPa
400 - 15000 psi
Average value: 33.1 MPa Grade Count:6
Users viewing this material also viewed the following: