Izod Impact, Notched (ISO) 129 kJ/m²
61.4 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12
LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.