Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.60 kJ/m² | 2.66 ft-lb/in² | Type A; ISO 180:2000 |
Nylacast Cast Nylon 6, Glass Filled Information provided by Nylacast Ltd. |
|||
Izod Impact, Notched (ISO) | 5.60 kJ/m² | 2.66 ft-lb/in² | Type A; ISO 180:2000 |
Nylacast PA6C Cast Nylon 6 Natural PA6 is the base to the other grades of material offered by Nylacast. It is available in Natural (off white) or Black colour. It is made by ionic polymerisation of e-caprolactam under anhydri.. |
|||
Izod Impact, Notched (ISO) | 5.60 kJ/m² | 2.66 ft-lb/in² | ISO 180 |
Polikim KESTAMID® PA6G Polyamide 6 Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical.. |
|||
Izod Impact, Notched (ISO) | 5.60 kJ/m² | 2.66 ft-lb/in² | Sample Type A; ISO 180:2000 |
Global EPP PA 6C Cast Polyamide 6 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Izod Impact, Notched (ISO) | 5.60 kJ/m² | 2.66 ft-lb/in² | ISO 180-93 |
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6 Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 5.60 kJ/m² | 2.66 ft-lb/in² | ISO 180 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Izod Impact, Notched (ISO) | 5.60 kJ/m² | 2.66 ft-lb/in² | ISO 180 |
Polikim KESTAMID® HS Polyamide 6, Heat Resistant Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with .. |
|||
Izod Impact, Notched (ISO) | 5.60 kJ/m² | 2.66 ft-lb/in² | ISO 180 |
BASF Ultramid® B3WG3 15% Glass Filled PA6 (Dry) Description: Ultramid B3WG3 is a 15% glass fiber reinforced, heat stabilized injection molding PA6 grade.Information provided by BASF |