Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with a longer duration compared to other extrusion and cast polyamide types. Its continuous operating temperature increases by 15-30°C compared to Kestamid® and reaches the 125-140°C interval. Thanks to its short term operating temperature that reaches 185-200°C interval, it is used safely in many applications that require heat resistance.Information provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption at Saturation 6.0 %
6.0 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ISO 868
Tensile Strength, Ultimate 78.5 MPa
11400 psi
ISO 527
Elongation at Break >= 20 %
>= 20 %
ISO 527
Tensile Modulus 4.00 GPa
580 ksi
ISO 527
Compressive Strength 93.2 MPa
13500 psi
ISO 604
Compressive Modulus 2.70 GPa
392 ksi
ISO 604
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
ISO 180
Charpy Impact Unnotched NB
NB
ISO 179
Coefficient of Friction 0.39
0.39
K Factor (Wear Factor) 0.44
0.44
[mg/km]
K (wear) Factor 500 x 10-8 mm³/N-M
248 x 10-10 in³-min/ft-lb-hr
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359
Melting Point 220 °C
428 °F
Maximum Service Temperature, Air 125 °C
257 °F
continuous
185 °C
365 °F
short term
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ISO 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO 60093
Dielectric Constant 3.7
3.7
ISO 60250
Dielectric Strength 25.0 kV/mm
635 kV/in
ISO 50243