Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.70 - 43.0 kJ/m²

@Temperature -40.0 - 10.0 °C
0.809 - 20.5 ft-lb/in²

@Temperature -40.0 - 50.0 °F
Average value: 5.81 kJ/m² Grade Count:31
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..