Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Mytex Polymers AS88L-01 Polypropylene, Compounded, Elastomer Description: AS88L-01 is a compounded, elastomer modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications .. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS PC/ABS with high stiffness and impact performance |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Asia Pacific) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature -30.0 °C |
21.4 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | ISO 180-1A |
Schwartz Technical Plastics LAMIGAMID® 410 Cast Polyamide 6, Elastomer Modified, Low Temp, Dry Application: outrigger floats, rollersInformation provided by Schwartz Technical Plastics GmbH |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 0.000 °C |
21.4 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 0.000 °C |
21.4 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp 2FL24 FP-E (EFTE) LNP* 2FL24 is a Fluoropolymer, ETFE grade containing Glass Fibers and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Izod Impact, Notched (ISO) | >= 45.0 kJ/m² | >= 21.4 ft-lb/in² | |
Sibur Discar-L PC/ABS Compositional Polymer Composition material PC/ABS with high shock resistance, thermal, light, and atmospheric resistance for structural parts of technical purpose and parts for internal finishing of automobiles. |
|||
Izod Impact, Notched (ISO) | >= 45.0 kJ/m² | >= 21.4 ft-lb/in² | |
Sibur Discar-SL PC/ABS Compositional Polymer Composition material PC/ABS with low viscosity of melting with high shock resistance, thermal and atmospheric resistance for large, thin wall structural parts of automobile interiors. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00AEU PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include : Easy Molding, UV Stabilized. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East) LNP* VERTON* Is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | ISO 180 |
Polyram RamLloy PBB704 PC/ABS Alloy, UV Stabilized PC/ABS alloy, UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | ISO 180/4A |
Chi Mei Wonderloy® PC-365 PC/ABS Alloy High Heat, High Impact |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² | 21.4 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Izod Impact, Notched (ISO) | 45.0 kJ/m² @Temperature 23.0 °C |
21.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermotuf P1000J5 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* P1000J5 is a compound based on PA 6 resin containing Impact Modifier.
Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |