Material Notes:
PC/ABS alloy, UV stabilized, for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ISO 2577
Melt Flow 18 g/10 min

@Load 5.00 kg,
Temperature 240 °C
18 g/10 min

@Load 11.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Tensile Modulus 2.00 GPa
290 ksi
ISO 527
Flexural Strength 80.0 MPa
11600 psi
ISO 178
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75
Vicat Softening Point 120 °C
248 °F
ISO 306
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Dielectric Strength 24.0 kV/mm
610 kV/in
IEC 60250