Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.50 - 47.0 kJ/m²
1.19 - 22.4 ft-lb/in²
Average value: 8.19 kJ/m² Grade Count:104
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched (ISO) 3.00 - 47.0 kJ/m²

@Temperature -30.0 - 0.000 °C
1.43 - 22.4 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 15.1 kJ/m² Grade Count:26
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched (ISO) 2.50 - 47.0 kJ/m²
1.19 - 22.4 ft-lb/in²
Average value: 14.3 kJ/m² Grade Count:111
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Izod Impact, Notched (ISO) 11.0 - 47.0 kJ/m²

@Temperature -40.0 - -20.0 °C
5.23 - 22.4 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 16.1 kJ/m² Grade Count:13
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..