Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 25.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 25.0 - 25.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 11.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 13.4 kJ/m² Grade Count:2
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched (ISO) 6.00 - 25.0 kJ/m²
2.86 - 11.9 ft-lb/in²
Average value: 12.3 kJ/m² Grade Count:13
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Izod Impact, Notched (ISO) 10.0 - 25.0 kJ/m²
4.76 - 11.9 ft-lb/in²
Average value: 20.0 kJ/m² Grade Count:3
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 6.00 - 25.0 kJ/m²
2.86 - 11.9 ft-lb/in²
Average value: 12.8 kJ/m² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Izod Impact, Notched (ISO) 5.00 - 25.0 kJ/m²
2.38 - 11.9 ft-lb/in²
Average value: 15.4 kJ/m² Grade Count:11
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched (ISO) 20.0 - 25.0 kJ/m²
9.52 - 11.9 ft-lb/in²
Average value: 23.3 kJ/m² Grade Count:3
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..
Copyright © lookpolymers.com All Rights Reserved