Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.00 - 28.0 kJ/m² | 4.28 - 13.3 ft-lb/in² | Average value: 16.6 kJ/m² Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Izod Impact, Notched (ISO) | 4.00 - 28.0 kJ/m² | 1.90 - 13.3 ft-lb/in² | Average value: 15.2 kJ/m² Grade Count:31 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Notched (ISO) | 2.40 - 28.0 kJ/m² | 1.14 - 13.3 ft-lb/in² | Average value: 8.43 kJ/m² Grade Count:14 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Izod Impact, Notched (ISO) | 16.0 - 28.0 kJ/m² | 7.61 - 13.3 ft-lb/in² | Average value: 20.7 kJ/m² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |