Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 3.30 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.30 - 3.30 kJ/m²

@Temperature -40.0 - -40.0 °C
1.57 - 1.57 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 3.30 kJ/m² Grade Count:1
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Izod Impact, Notched (ISO) 3.30 kJ/m²

@Thickness >=5.00 mm
1.57 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola
Izod Impact, Notched (ISO) 3.30 kJ/m²

@Thickness >=5.00 mm
1.57 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Elektro-Isola Etronit IIQ R Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Izod Impact, Notched (ISO) 3.30 kJ/m²

@Thickness >=5.00 mm
1.57 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets
Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition..
Izod Impact, Notched (ISO) 3.30 kJ/m²

@Thickness >=5.00 mm
1.57 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart..
Izod Impact, Notched (ISO) 3.30 kJ/m²

@Thickness >=5.00 mm
1.57 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets
Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T..
Izod Impact, Notched (ISO) 3.30 kJ/m²
1.57 ft-lb/in²
ISO 180/1A
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot..