Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 66.0 kJ/m² | 31.4 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 236SI PA6, DRY Description: Unreinforced polyamide 6 with high impact strength for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® C 236SI has high impact strength and fle.. |
|||
Izod Impact, Notched (ISO) | 66.0 kJ/m² | 31.4 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |