Izod Impact, Notched (ISO) 11.2 kJ/m²
5.33 ft-lb/in²
ISO 180
LNP Thermocomp® LF-1006 EM Polyetheretherketone, Glass Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Izod Impact, Notched (ISO) 11.2 kJ/m²
5.33 ft-lb/in²
ISO Test
BASF Ultramid® B3WG7 BK00564 35% Glass Filled PA6 (Dry)
Ultramid B3WG7 BK00564 is a 35% glass fiber reinforced, pigmented black, injection molding PA6 grade for highly rigid, dimensionally stable components which are resistant to high temperature aging a..