Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.90 kJ/m² | 2.81 ft-lb/in² | ISO 180/1A |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Izod Impact, Notched (ISO) | 5.90 kJ/m² | 2.81 ft-lb/in² | ISO Test |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |