Izod Impact, Notched (ISO) 6.40 - 50.0 kJ/m²
3.05 - 23.8 ft-lb/in²
Average value: 33.0 kJ/m² Grade Count:13
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Izod Impact, Notched (ISO) 10.0 - 50.0 kJ/m²
4.76 - 23.8 ft-lb/in²
Average value: 19.1 kJ/m² Grade Count:23
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched (ISO) 3.00 - 50.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 23.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 9.42 kJ/m² Grade Count:39
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..