Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.00 - 54.6 kJ/m²
3.33 - 26.0 ft-lb/in²
Average value: 10.7 kJ/m² Grade Count:24
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..