Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.34 - 1.75 g/cc
0.0484 - 0.0632 lb/in³
Average value: 1.51 g/cc Grade Count:91
Filler Content 20.0 - 33.0 %
20.0 - 33.0 %
Average value: 31.0 % Grade Count:61
Water Absorption 0.0200 - 5.00 %
0.0200 - 5.00 %
Average value: 0.377 % Grade Count:43
1.25 - 1.35 %

@Temperature 70.0 - 70.0 °C
1.25 - 1.35 %

@Temperature 158 - 158 °F
Average value: 1.30 % Grade Count:4
Moisture Absorption at Equilibrium 0.100 - 1.70 %
0.100 - 1.70 %
Average value: 0.900 % Grade Count:5
Additive Loading 30.0 %
30.0 %
Average value: 30.0 % Grade Count:3
Linear Mold Shrinkage 0.000 - 0.0100 cm/cm
0.000 - 0.0100 in/in
Average value: 0.00385 cm/cm Grade Count:79
Linear Mold Shrinkage, Transverse 0.00200 - 0.0130 cm/cm
0.00200 - 0.0130 in/in
Average value: 0.00812 cm/cm Grade Count:47
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121 - 125
121 - 125
Average value: 125 Grade Count:15
Ball Indentation Hardness 270 - 290 MPa
39200 - 42100 psi
Average value: 283 MPa Grade Count:3
Tensile Strength, Ultimate 68.9 - 233 MPa
10000 - 33800 psi
Average value: 176 MPa Grade Count:81
60.0 - 150 MPa

@Temperature 60.0 - 230 °C
8700 - 21800 psi

@Temperature 140 - 446 °F
Average value: 100 MPa Grade Count:8
100 - 107.5 MPa

@Temperature 130 - 180 °C
14500 - 15590 psi

@Temperature 266 - 356 °F
Average value: 100 MPa Grade Count:4
100 - 107.5 MPa

@Time 1.80e+7 - 7.20e+7 sec
14500 - 15590 psi

@Time 5000 - 20000 hour
Average value: 100 MPa Grade Count:4
Tensile Strength, Yield 145 - 225 MPa
21000 - 32600 psi
Average value: 186 MPa Grade Count:10
63.4 - 119 MPa

@Temperature 100 - 175 °C
9200 - 17300 psi

@Temperature 212 - 347 °F
Average value: 87.2 MPa Grade Count:3
Elongation at Break 1.00 - 4.00 %
1.00 - 4.00 %
Average value: 2.14 % Grade Count:86
1.50 - 9.00 %

@Temperature 60.0 - 230 °C
1.50 - 9.00 %

@Temperature 140 - 446 °F
Average value: 5.11 % Grade Count:11
Modulus of Elasticity 7.58 - 18.6 GPa
1100 - 2700 ksi
Average value: 12.1 GPa Grade Count:79
4.30 - 11.5 GPa

@Temperature 60.0 - 175 °C
624 - 1670 ksi

@Temperature 140 - 347 °F
Average value: 6.88 GPa Grade Count:10
Flexural Yield Strength 103 - 326 MPa
15000 - 47300 psi
Average value: 254 MPa Grade Count:78
80.0 - 227 MPa

@Temperature 100 - 175 °C
11600 - 32900 psi

@Temperature 212 - 347 °F
Average value: 129 MPa Grade Count:8
Flexural Modulus 7.58 - 14.1 GPa
1100 - 2050 ksi
Average value: 11.0 GPa Grade Count:78
3.60 - 9.80 GPa

@Temperature 100 - 175 °C
522 - 1420 ksi

@Temperature 212 - 347 °F
Average value: 5.87 GPa Grade Count:8
Compressive Yield Strength 145 - 276 MPa
21000 - 40000 psi
Average value: 185 MPa Grade Count:14
Poissons Ratio 0.370 - 0.410
0.370 - 0.410
Average value: 0.406 Grade Count:10
Shear Modulus 4.15 - 5.18 GPa
602 - 751 ksi
Average value: 4.58 GPa Grade Count:3
Shear Strength 62.1 - 101 MPa
9010 - 14600 psi
Average value: 85.4 MPa Grade Count:17
Izod Impact, Notched 0.370 - 1.33 J/cm
0.693 - 2.50 ft-lb/in
Average value: 0.793 J/cm Grade Count:56
Izod Impact, Unnotched 1.60 - 14.0 J/cm
3.00 - 26.2 ft-lb/in
Average value: 6.57 J/cm Grade Count:38
Izod Impact, Notched (ISO) 7.00 - 54.6 kJ/m²
3.33 - 26.0 ft-lb/in²
Average value: 10.7 kJ/m² Grade Count:24
7.00 - 10.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.33 - 4.76 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 40.0 - 68.0 kJ/m²
19.0 - 32.4 ft-lb/in²
Average value: 50.7 kJ/m² Grade Count:13
37.0 - 37.0 kJ/m²

@Temperature -30.0 - -30.0 °C
17.6 - 17.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 37.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 3.00 - 9.70 J/cm²
14.3 - 46.2 ft-lb/in²
Average value: 5.65 J/cm² Grade Count:29
3.50 - 5.00 J/cm²

@Temperature -40.0 - -30.0 °C
16.7 - 23.8 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.05 J/cm² Grade Count:6
Charpy Impact, Notched 0.600 - 1.40 J/cm²
2.86 - 6.66 ft-lb/in²
Average value: 0.929 J/cm² Grade Count:32
0.700 - 2.10 J/cm²

@Temperature -40.0 - -30.0 °C
3.33 - 9.99 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.972 J/cm² Grade Count:7
Thermal Properties Metric English Comments
CTE, linear 17.0 - 72.0 µm/m-°C
9.44 - 40.0 µin/in-°F
Average value: 23.9 µm/m-°C Grade Count:24
7.00 - 100 µm/m-°C

@Temperature 55.0 - 250 °C
3.89 - 55.6 µin/in-°F

@Temperature 131 - 482 °F
Average value: 20.4 µm/m-°C Grade Count:19
CTE, linear, Transverse to Flow 45.0 - 80.0 µm/m-°C
25.0 - 44.4 µin/in-°F
Average value: 62.8 µm/m-°C Grade Count:18
Electrical Properties Metric English Comments
Electrical Resistivity 1000 - 1.00e+17 ohm-cm
1000 - 1.00e+17 ohm-cm
Average value: 5.41e+15 ohm-cm Grade Count:48
Surface Resistance 1.00e+6 - 2.00e+16 ohm
1.00e+6 - 2.00e+16 ohm
Average value: 2.84e+15 ohm Grade Count:12
Dielectric Constant 3.30 - 5.50
3.30 - 5.50
Average value: 4.08 Grade Count:26
Dielectric Strength 18.0 - 36.0 kV/mm
457 - 914 kV/in
Average value: 22.7 kV/mm Grade Count:29
Dissipation Factor 0.00400 - 0.0220
0.00400 - 0.0220
Average value: 0.0117 Grade Count:26
Arc Resistance 120 - 300 sec
120 - 300 sec
Average value: 169 sec Grade Count:8
Comparative Tracking Index 175 - 600 V
175 - 600 V
Average value: 567 V Grade Count:32
Hot Wire Ignition, HWI 60.0 - 150 sec
60.0 - 150 sec
Average value: 120 sec Grade Count:4
High Amp Arc Ignition, HAI 74.0 - 120 arcs
74.0 - 120 arcs
Average value: 109 arcs Grade Count:4
High Voltage Arc-Tracking Rate, HVTR 0.000 - 18.0 mm/min
0.000 - 0.709 in/min
Average value: 14.8 mm/min Grade Count:11
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved