Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.00 - 55.0 kJ/m² | 3.81 - 26.2 ft-lb/in² | Average value: 19.9 kJ/m² Grade Count:9 |
Overview of materials for Phenolic, Novolac, Fabric Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched (ISO) | 5.30 - 55.0 kJ/m² | 2.52 - 26.2 ft-lb/in² | Average value: 15.7 kJ/m² Grade Count:28 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |