Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Extem UH1016M TPI Blend
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
FG20GT NC010 PCT  (discontinued **)
Thermx® FG20GT NC010 is a 20% glass fiber reinforced, toughened modified polycyclohexylenedimethylene terephthalate resin suitable for repeated-use food-contact US FDA housewares applications.Celen..
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180/1A
S471 LCP, 45% Mineral / Glass Reinforced  (Unverified Data**)
High flow, High Heat resistance, Low Warpage, for Thick Walled (>0.2mm) or thin (
Izod Impact, Notched (ISO) 8.00 - 55.0 kJ/m²
3.81 - 26.2 ft-lb/in²
Average value: 19.9 kJ/m² Grade Count:9
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched (ISO) 8.00 - 64.0 kJ/m²

@Temperature -40.0 - -20.0 °C
3.81 - 30.5 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 13.3 kJ/m² Grade Count:45
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180-1A
Gromax BBG30-AN00N1 Nylon 6, Flame Retardant (Dry)
Information provided by Gromax Enterprises Corp.
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP RFL25ES PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL25ES is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Easy Molding.
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-KON DEL13PXC PC (Europe-Africa-Middle East)
LNP* Stat-kon* DEL13PXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Superior Molding.
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® 420 PBT
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Europe-Africa-Middle East)
LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East)
Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production..
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF002S is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Heat Stabilized.
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180-93
Wellman Wellamid® FRGF1850-BK1 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
All information provided by Wellman Engineered Resins.
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180-93
Wellman Wellamid® FRGFT1741-BK2 Nylon 66, 32% Glass Fiber Reinforced, Flame Retardant
All information provided by Wellman Engineered Resins.
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180/1A
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene
POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w..
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
Low Temp; ISO 180/A
CTC SunPro® SP 200 P3081 Polypropylene Copolymer
SunPro® SP 200 P 3081 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM PP ..
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80x10x4; ISO 179/1eA
Eurostar Staramide RF003S PA66, 15% Glass Fiber Filled, Injection Molded
Staramide RF003S is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180/1A
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -40.0 - -40.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 8.00 kJ/m² Grade Count:2
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics XYLEX X8300CL PC+POLYESTER (Europe-Africa-Middle East)
PC+Polyester, UV Stabilized, Transparent, OQ Quality
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180
LNP Thermocomp® SPS-F-1006 HS Syndiotactic Polystyrene, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..
Copyright © lookpolymers.com All Rights Reserved