Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.00 - 6.20 kJ/m²
1.43 - 2.95 ft-lb/in²
Average value: 4.92 kJ/m² Grade Count:13
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..