Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 4.80 - 6.30 kJ/m² @Temperature -40.0 - -40.0 °C |
2.28 - 3.00 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 5.44 kJ/m² Grade Count:7 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched (ISO) | 3.00 - 6.30 kJ/m² | 1.43 - 3.00 ft-lb/in² | Average value: 4.95 kJ/m² Grade Count:6 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |