Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 15.5 - 16.5 kJ/m² | 7.38 - 7.85 ft-lb/in² | ASTM D256 |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |
|||
Izod Impact, Notched (ISO) | 15.5 kJ/m² | 7.38 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® CR 218 V33 Black 21 N Nylon 6, 30% glass fiber, DRY Description: Polyamide PA6 reinforced with 33% of glass fiber, heat stabilized, containing recycled material.Available in: North AmericaProduct Applications: This grade is suitable for none critical.. |
|||
Izod Impact, Notched (ISO) | 15.5 kJ/m² | 7.38 ft-lb/in² | ISO 180 |
Polyram RamOfin PPH343T8 Polypropylene, 40% Mineral Filled 40% Mineral filled polypropylene for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 15.5 kJ/m² | 7.38 ft-lb/in² | ISO 180/A |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Izod Impact, Notched (ISO) | 15.5 kJ/m² @Temperature 23.0 °C |
7.38 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned) Description: 30% glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of high stiffness and dimensional stability such as lamp socket housings, f.. |