Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamOfin PPH343T8 Polypropylene, 40% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamOfin PPH343T8 Polypropylene, 40% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Mineral filled polypropylene for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0070 - 0.011 cm/cm
0.0070 - 0.011 in/in
ISO 2577
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Tensile Modulus 3.60 GPa
522 ksi
ISO 527
Flexural Strength 50.0 MPa
7250 psi
ISO 178
Flexural Modulus 3.80 GPa
551 ksi
ISO 178
Izod Impact, Notched (ISO) 15.5 kJ/m²
7.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 168 °C
334 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Flame Spread 22 mm/min
0.87 in/min
FMVSS302