Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 800 kg | 1760 lb (mass) | ASTM D2596, DIN 51 350 |
Chesterton 783 ACR Anti-Seize Compound Description: Chesterton® 783 ACR represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants, 783 ACR can be used under extremely severe co.. |
|||
Four Ball Extreme Pressure, Weld Load | 800 kg | 1760 lb (mass) | ASTM D2596, DIN 51 350/4 |
Chesterton 633 SXCM Synthetic, Extreme Pressure & Corrosion Resistant Grease-with Moly Description: Chesterton® 633 Synthetic Extreme Pressure & Corrosion Resistant Grease with Moly is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse wit.. |
|||
Four Ball Extreme Pressure, Weld Load | 800 kg | 1760 lb (mass) | ASTM D2596, DIN 51 350/4 |
Chesterton 635 SXC Synthetic, Extreme Pressure & Corrosion Resistant Grease Description: Chesterton® Synthetic Extreme Pressure & Corrosion Resistant Grease is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse with outstanding .. |