Material Notes:
Description: Chesterton® Synthetic Extreme Pressure & Corrosion Resistant Grease is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse with outstanding extreme pressure and anti-wear capabilities, shear stability, temperature and corrosion resistance. Superior resistance to washout by water, caustics, and acids, sanitizing cleaners, process fluids and steam has now been combined with high temperature performance to produce Chesterton 635 Synthetic Extreme Pressure & Corrosion Resistant Grease. As a premium quality, water resistant grease, 635 will not be removed even in severe water washout situations. Chesterton 635 can be used in steam and direct water contact services. Up to 50% water contamination will not diminish properties of Chesterton 635. With a dropping point of 318°C (604°F), it will not melt and run out even at high speeds or under heavy loads. 635 SXC has great ability to extend bearing life, reduce equipment repairs and improve operational efficiency of grease lubricated equipment. Uses for 635 SXC can be found throughout any industrial plant or process. It is especially advantageous where there is exposure to high humidity, corrosive vapors and shock loading or vibration as found in pulp and paper mills, mining operations, power generating plants, steel mills and metal forming operations. Applications include the lubrication of pinch roll and press roll bearings, oven conveyors bearings, cranes and mechanical presses. Features: Virtually impervious to water and steamSynthetic Base FluidCompatible with most elastomers and seals. Smooth, Buttery TextureAdheres to MetalWater and Corrosion ResistantWide application temperature rangeSpeed Rating, DN to 500,000.Sugested Uses: Use in all applications where conventional greases break down under shear, thermal abuse, shock loading and water contamination. Chesterton 635 SXC can be used wherever thermally stable grease is required.Applications:Lubriation of slides, guides, plain bearings and bushingsAnti-friction bearings, roller bearings, and ball bearingsGrease-lubricated chainsGears, cams, ball screw actuatorsMotor Operated Valves, Limit Switch and stem NutCouplings, joints and splined shaftsMachine tool spindlesLubricating Additives: Non Heavy Metal, Extreme Pressure and Anti-Wear, Anti-Fretting Additives, Surface Reactive Anti-Rust and Corrosion Additives, Oxidation InhibitorsInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.950 - 1.05 g/cc
0.950 - 1.05 g/cc
Viscosity Measurement 146
146
Base Oil; ASTM D445
Kinematic Viscosity at 40°C (104°F) 98 cSt
98 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 14 cSt
14 cSt
Base Oil; ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 130
130
ASTM D2596, DIN 51 350/4
Four Ball Extreme Pressure, Weld Load 800 kg
1760 lb (mass)
ASTM D2596, DIN 51 350/4
Four Ball Wear 0.400 mm

@Temperature 75.0 °C,
Time 3600 sec
0.0157 in

@Temperature 167 °F,
Time 1.00 hour
1200 rpm, 40 kg, scar diameter; ASTM D2266, DIN 51 350/5
Penetration 265 - 295
265 - 295
ASTM D217, DIN ISO 2137
Timken Test 29500 g
65.0 lb
ASTM D2509
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 240 °C
464 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Dropping Point 318 °C
604 °F
ASTM D2265, DIN 51 801/1
Descriptive Properties Value Comments
Bearing Life 240 hrs
ASTM D3527
Bomb Oxidation 6 psi drop
1000 hrs, ASTM D942
Color Light Blue/Green
Consistency 2
NLGI, DIN 51 818
Copper Corrosion 0/1B
ASTM D4048, DIN 51 811
Corrosion Resistance >1000 hrs
@ 50 microns film thickness, 5% NaCl, ASTM B117
Oil Base PAO Synthetic
Texture Smooth, Buttery
Thickener Proprietary, Patent Protected, Sulfonate Complex
Water Washout Resistance <0.05%
@79°C, ASTM D1264
Worked Stability -0.01
10000 Strokes, ASTM D217
-0.045
10000 Strokes, ASTM D217