Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2596 |
ExxonMobil 1 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Extreme Pressure, Weld Load | >= 200 kg | >= 441 lb (mass) | ASTM D2596 |
ExxonMobil 100 Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2596 |
ExxonMobil 2 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Extreme Pressure, Weld Load | >= 200 kg | >= 441 lb (mass) | ASTM D2596 |
ExxonMobil 32 Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2596 |
ExxonMobil 78 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2783 |
ExxonMobil Mobil Vactra 3 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2783 |
ExxonMobil Mobil Vactra 4 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | |
ELM® SoyGrease™ Premium Biodegradable Food Grade Grease, NLGI Grade 2 Description: Elm ELM SoyGrease™ Food Machinery is formulated with optimized USA grown natural seed oils that surpass the lubricity of most conventional oils. It is formulated in accordance with th.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2596 |
ExxonMobil 1 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2596 |
ExxonMobil 2 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Extreme Pressure, Weld Load | >= 200 kg | >= 441 lb (mass) | ASTM D2596 |
ExxonMobil 32 Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2596 |
ExxonMobil 78 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2783 |
ExxonMobil Mobil Vactra 1 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2783 |
ExxonMobil Mobil Vactra 2 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2783 |
ExxonMobil Mobil Vactra 3 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2783 |
ExxonMobil Mobil Vactra 4 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D-2596 |
ConocoPhillips Grade 2 Calcium S Grease NLGI Description: Conoco Calcium S Grease is a light, specialty calcium stearate thickened product that is used in the automotive assembly industry. It is amber in color and is used in applications where.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | |
ELM® SoyGrease™ Premium Biodegradable Food Grade Grease, NLGI Grade 1 Description: Elm ELM SoyGrease™ Food Machinery is formulated with optimized USA grown natural seed oils that surpass the lubricity of most conventional oils. It is formulated in accordance with th.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | Weld Point |
ChevronTexaco Delo® Synthetic Grease SF FeaturesChevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperature.. |
|||
Four Ball Extreme Pressure, Weld Load | >= 200 kg | >= 441 lb (mass) | ASTM D2596 |
ExxonMobil 100 Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2783 |
ExxonMobil Mobil Vactra 1 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Four Ball Extreme Pressure, Weld Load | 200 kg | 441 lb (mass) | ASTM D2783 |
ExxonMobil Mobil Vactra 2 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |