Polymer Property : Four Ball Extreme Pressure, Weld Load = 441 lb (mass) Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2596
ExxonMobil 1 Mobiltemp Series
Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con..
Four Ball Extreme Pressure, Weld Load >= 200 kg
>= 441 lb (mass)
ASTM D2596
ExxonMobil 100 Mobiltemp SHC Series
Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base ..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2596
ExxonMobil 2 Mobiltemp Series
Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con..
Four Ball Extreme Pressure, Weld Load >= 200 kg
>= 441 lb (mass)
ASTM D2596
ExxonMobil 32 Mobiltemp SHC Series
Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base ..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2596
ExxonMobil 78 Mobiltemp Series
Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2783
ExxonMobil Mobil Vactra 3
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2783
ExxonMobil Mobil Vactra 4
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ELM® SoyGrease™ Premium Biodegradable Food Grade Grease, NLGI Grade 2
Description: Elm ELM SoyGrease™ Food Machinery is formulated with optimized USA grown natural seed oils that surpass the lubricity of most conventional oils. It is formulated in accordance with th..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2596
ExxonMobil 1 Mobiltemp Series
Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2596
ExxonMobil 2 Mobiltemp Series
Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con..
Four Ball Extreme Pressure, Weld Load >= 200 kg
>= 441 lb (mass)
ASTM D2596
ExxonMobil 32 Mobiltemp SHC Series
Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base ..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2596
ExxonMobil 78 Mobiltemp Series
Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2783
ExxonMobil Mobil Vactra 1
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2783
ExxonMobil Mobil Vactra 2
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2783
ExxonMobil Mobil Vactra 3
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2783
ExxonMobil Mobil Vactra 4
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D-2596
ConocoPhillips Grade 2 Calcium S Grease NLGI
Description: Conoco Calcium S Grease is a light, specialty calcium stearate thickened product that is used in the automotive assembly industry. It is amber in color and is used in applications where..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ELM® SoyGrease™ Premium Biodegradable Food Grade Grease, NLGI Grade 1
Description: Elm ELM SoyGrease™ Food Machinery is formulated with optimized USA grown natural seed oils that surpass the lubricity of most conventional oils. It is formulated in accordance with th..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
Weld Point
ChevronTexaco Delo® Synthetic Grease SF
FeaturesChevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperature..
Four Ball Extreme Pressure, Weld Load >= 200 kg
>= 441 lb (mass)
ASTM D2596
ExxonMobil 100 Mobiltemp SHC Series
Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base ..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2783
ExxonMobil Mobil Vactra 1
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a..
Four Ball Extreme Pressure, Weld Load 200 kg
441 lb (mass)
ASTM D2783
ExxonMobil Mobil Vactra 2
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a..