Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 251 kg
553 lb (mass)
Init. Seiz. Load; IP 239
Solvay Specialty Polymers FOMBLIN® Y45 PFPE Lubricant